Abstract

Tanaman pinang sirih (Areca catechu L.) adalah sejenis palma yang dimanfaatkan untuk tujuan komersial karena memiliki nilai ekonomis yang tinggi pada setiap bagian dari tanaman pinang mulai dari daun, batang, biji dan serabut. Bagian dari tanaman pinang yang belum dimanfaatkan secara maksimal terletak pada serat yang terdapat pada buah tanaman pinang. Serat pinang mengandung selulosa sebesar 53,2%, sehingga berpotensi untuk dimanfaatkan sebagai bahan baku pembuatan pulp untuk kertas seni. Pada pembuatan kertas seni untuk memperoleh warna yang lebih cerah, diperlukan proses pemutihan untuk menarik perhatian ketika dilihat. Pada saat proses pemutihan faktor yang harus diperhatikan yaitu kadar bahan kimia untuk pemutih dan lama waktu saat proses pemutihan. Tujuan penelitian ini adalah mengetahui penambahan kadar H2O2 dan lama waktu pemasakan bleaching yang optimal pada pembuatan kertas dari serat pinang dan kertas kardus bekas untuk menghasilkan kertas seni yang berkualitas dari segi fisik kertas yaitu kuat tarik, tebal kertas, gramatur dan kecerahan. Metode RSM merupakan kumpulan teknik statistik dan matematis yang digunakan untuk mengembangkan, memperbaiki dan mengoptimalkan proses, dimana respon yang ditentukan dipengaruhi oleh beberapa variabel yang bertujuan untuk mengoptimalkan respon yang telah ditentukan. Metode ini dapat diterapkan pada proses kimia. Model yang digunakan dalam RSM yaitu CCD (Central Design Composite) dengan menggunakan 2 faktor perlakuan, yaitu faktor pertama adalah lama waktu bleaching (X1) dan faktor kedua adalah kadar H2O2 (X2). Faktor pertama menggunakan batas atas 90 menit (X1=-1) dan batas bawah 150 menit (X1=1). Faktor kedua menggunakan viii batas atas 5% (X1=-1) dan batas bawah 15% (X1=1). Respon yang akan diuji yaitu kuat tarik dan tingkat kecerahan. Pada kombinasi perlakuan lama waktu bleaching dan kadar H2O2 didapatkan perlakuan terbaik yaitu lama waktu bleaching 150 menit dan kadar H2O2 15%. Hasil respon optimal yang didapatkan yaitu tingkat kecerahan 69,50% dan kuat tarik 14,71 kN/m2. Hasil uji fisik kertas seni lainnya yaitu gramatur 282 gr/cm2, ketebalan 0,88 mm dan kadar air 6,5%.

English Abstract

Betel plant (Areca catechu L.) is a type of palm that is used for commercial purposes because it has high economic value in every part of the areca nut plant starting from leaves, stems, seeds and fibers. Part of the areca nut that has not been used optimally lies in the fiber found in the areca nut. Areca nut contains cellulose of 53.2%, so it has the potential to be used as raw material for pulp making for paper craft. In making paper craft to obtain brighter colors, bleaching process is needed to attract attention when viewed. During the bleaching process the factors that must be considered are the levels of chemicals for bleach and the length of time during the bleaching process. The purpose of this study was to determine the addition of H2O2 levels and the length of time for optimal bleaching in the manufacture of paper from areca fibers and used cardboard paper to produce quality paper craft in terms of physical paper, namely tensile strength, paper thickness, grammar and brightness. Response surface method (RSM) is a collection of statistical and mathematical techniques that are used to develop, improve and optimize the process, where the response is determined to be influenced by several variables that aim to optimize the predetermined response. This method can be applied to chemical processes. The model used in RSM is CCD (Central Design Composite) using 2 treatment factors, namely the first factor is the length of bleaching time (X1) and the second factor is H2O2 (X2). The first factor uses an upper limit of 90 minutes (X1 = -1) and a lower limit of 150 minutes (X1 = 1). The second factor uses the upper limit of 5% (X1 = -1) and the lower limit of x 15% (X1 = 1). The response to be tested is tensile strength and brightness level. In the combination treatment of bleaching time and H2O2, the best treatment was 150 minutes and 15% H2O2. The optimal response results obtained are 69.50% brightness and 14.71 kN/m2 tensile strength. Other physical test results of art paper are 282 gr/cm2, 0.88 mm thickness and 6.5% moisture content.

Item Type: Thesis (Sarjana)
Identification Number: SKR/FTP/2018/493/051810334
Uncontrolled Keywords: H2O2, Kertas Seni, Response Surface Method, Serat Pinang Sirih,/ Areca Nut Fiber, H2O2, Paper Craft, Response Surface Method
Subjects: 600 Technology (Applied sciences) > 676 Pulp and paper technology
Divisions: Fakultas Teknologi Pertanian > Teknologi Industri Pertanian
Depositing User: Endang Susworini
Date Deposited: 17 Oct 2019 08:11
Last Modified: 23 Nov 2021 05:38
URI: http://repository.ub.ac.id/id/eprint/164945
[thumbnail of Dendis Elfiska Royyani.pdf]
Preview
Text
Dendis Elfiska Royyani.pdf

Download (3MB) | Preview

Actions (login required)

View Item View Item